ECO - IRON ADAL TABLET

ECO - IRON ADAL TABLET

General Description :
ECO – Fe ADAL TABLET are used to adjust and compound the content of Fe in Aluminium alloy and to replace Al-Fe alloy. ECO – Fe ADAL TABLET are light grey in color.

Instruction :
1. When the temperature of melt reaches 730-7600C, skim the slag off.
2. Add demanded additive, wait for 10 minutes and stir completely. (If the melt is dirty, should refine again and deslag, and then add the additive to improve the recovery.)

Application Rate :
Added volume = Needed volume in Al alloys / 75% (80%) X 90%(recovery percentage)
Note : The recovery of 75 FeAl or 80FeAl can reach 95%

ECO – Fe ADITIVE: 75 FeF/80FeF/75FeAl/80FeAl

  • Easy for operation to reduce labor intensity
  • It can avoid the oxide and the salt inclusion can purify the melt
  • FeAl additive is high grade product with the special feature of quick melting speed and high recovery.

Feature Products

Get a Quote

Please enable JavaScript in your browser to complete this form.

Storage :
Store in dry warehouse. Avoid contact with moisture.

Valid Date :

6 months

Material Safety Data :

Appearance : Light grey tablet
Density : > 3.9g/cm3
Color code label : Gree